Comparison of a new, green foundry binder with conventional foundry binders
RESEARCH
Comparison of a new, green foundry binder with conventional foundry binders
01 Jan 2012
Contributors:
… that matched or exceeded those of conventional phenolic urethane. Also, in iron erosion … into an aluminum pan and dried at 110 C for 12 h. For the conventional phenolic urethane, …